Friday, June 20, 2008

Calcined Zinc


Something we crystal-glazers get up to: the raw crystal-glaze layer needs to be thick [2-4mm.] and calcining the Zinc [firing to 900-odd degrees] prevents cracking,peeling,shedding and other undesirable and troublesome manifestations. I do it in bisced bowls at the bottom of the bisc kiln.